Permabond LH056 Anaerobic Threadsealant

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond LH056 Anaerobic Threadsealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond LH056 is a thread sealant designed for use in sealing metal pipes and fittings in sprinkler systems which may also contain CPVC piping. Permabond LH056 prevents leaks even on pipes that are not completely seated.  This anaerobically curing thread sealant forms an instant seal.  Once fully cured, the seal will generally surpass the burst rating of most piping systems. In addition, it locks the pipes, plugs, or fittings against vibration loosening, tampering, and variable temperature effects. Permabond LH056 is FBCTM System Compatible. Features & Benefits: Instant pressure seal Seals to burst rating of pipe Slow curing – allows accurate adjustment Information provided by Permabond.
Physical Properties Metric English Comments
Viscosity 90000 - 150000 cP

@Temperature 25.0 °C
90000 - 150000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min

@Temperature 23.0 °C
0.500 - 1.00 hour

@Temperature 73.4 °F
brass, fixture time
60.0 - 120 min

@Temperature 23.0 °C
1.00 - 2.00 hour

@Temperature 73.4 °F
black iron, fixture time
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
full strength
Descriptive Properties Value Comments
Appearance White
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 50% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 3
M10 steel, prevail
6
M10 steel, break