Permabond CSA-NF Cyanoacrylate Surface Activator

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond CSA-NF Cyanoacrylate Surface Activator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond C Surface Activator (CSA-NF) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It significantly reduces the whitening effect often associated with more active cyanoacrylates. It has been developed to be non-harmful and non-flammable making storage, shipment and use of the product less hazardous. Use of CSA-NF enables fillets of cured adhesive to be formed if required and can be used to reduce the effects of blooming, which can affect black or decorative surfaces. Also, it facilitates the bonding of porous surfaces. Features & Benefits: Non-flammable Non-blooming Activates difficult or porous surfaces Improves adhesive gap fill Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Uncured
Viscosity 1.0 cP
1.0 cP
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Thermal Properties Metric English Comments
Boiling Point 40.0 °C
104 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless