Permabond ASC10 Anaerobic Surface Conditioner

Category Fluid , Solvent
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond ASC10 Anaerobic Surface Conditioner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND ASC10 Anaerobic Conditioner is a rapid drying accelerator for use with PERMABOND Anaerobic Adhesive/Sealants. It is designed to be used primarily on inactive surfaces such as zinc plating, cadmium plating, passivated stainless steel, gold, glass, plastic and painted surfaces. It improves the cure of anaerobic adhesives on poorly mated parts. It can also be used to increase the cure rate on less active substrates such as aluminum. This product contains a non-halogenated solvent that is not ozone depleting. Evaporation leaves a thin deposit of initiator on the surface to be bonded. Parts can be activated up to 30 days before bonding. FEATURES & BENEFITS: Contains no ozone depleting agent Rapid drying Faster cure on a variety of surfaces Helps remove contaminants from surfaces Improves cure speed at low temperatures Enables cure to take place on painted surfaces Improves cure on poorly mated parts TYPICAL APPLICATIONS: Plated Screws Plated Weld Nuts Aluminum Parts-Where Faster Cure is required Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 0.730 g/cc
0.730 g/cc
Thermal Properties Metric English Comments
Flash Point -7.00 °C
19.4 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Blue Green