Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond A136 Anaerobic Gasketmaker

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond A136 Anaerobic Gasketmaker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potential for reduced stock holdings. By allowing surface to surface contact, load transmission can be improved. As the product does not shrink, creep or relax after curing, no bolt re-tightening is required. Its excellent chemical resistance allows its use with a wide variety of gases and liquids. Features & Benefits: Does not creep or shrink Improved stress distribution No shimming effect No loose particles to clog oilways etc. WRAS listed for contact with wholesome (potable) waterInformation provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 18000 cP

@Temperature 25.0 °C
18000 cP

@Temperature 77.0 °F
at 20 rpm vibration
75000 cP

@Temperature 25.0 °C
75000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 12.0 MPa
1740 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, working strength
<= 30.0 min

@Temperature 23.0 °C
<= 0.500 hour

@Temperature 73.4 °F
M10 steel, handling strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, handling strength
120 min

@Temperature 23.0 °C
2.00 hour

@Temperature 73.4 °F
M10 steel, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
420 min

@Temperature 23.0 °C
7.00 hour

@Temperature 73.4 °F
Zinc, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Red
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 20% at 150°C
Relative to 0°C
70% at 100°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Torque Strength (N m) 10
M10 steel, break
8
M10 steel, prevail
UV Fluorescence Yes
Uncured
Copyright © lookpolymers.com All Rights Reserved