Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond A025 Anaerobic Retainer

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond A025 Anaerobic Retainer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for applications where joints have to withstand temperatures up to 200°C or where the maximum degree of chemical resistance is required. These features allow machining tolerances to be relaxed and mechanical locking devices to be eliminated, with consequent cost savings. Features & Benefits: Excellent temperature resistance Excellent chemical resistance WRAS listed for contact with wholesome (potable) water. Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 750 cP

@Temperature 25.0 °C
750 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.00 MPa
1160 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 - 30.0 min

@Temperature 23.0 °C
0.250 - 0.500 hour

@Temperature 73.4 °F
M10 steel, handling strength
120 min

@Temperature 23.0 °C
2.00 hour

@Temperature 73.4 °F
M10 steel, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Orange
Uncured
Maximum Gap Fill (mm) 0.2
Maximum Thread Size M20
Strength Retention 20% at 250°C
Relative to 0°C
70% at 200°C
Relative to 0°C
88% at 150°C
Relative to 0°C
92% at 100°C
Relative to 0°C
96% at 50°C
Relative to 0°C
Torque Strength (N m) 13
M10 steel, break
23
M10 steel, prevail
UV Fluorescence Yes
Uncured