Material Notes:
Specially developed for high temperature (HT)dcables.Imparts very good electrical insulation resistance in addition to ling term heat stability and ageing resistance as well as the low water absorption.Unistab ECZ-660 is also excellent for the stabilization of flame retardant formulations.Information provided by Pau Tai Industrial Corp.Advantages: Decreases fusion time of rigid PVC compoundsProduces highly homogeneous meltsPromotes smooth processing of PVC in processing machinery.Gives excellent hot strength, cohesion, rolling bank, and well-knit edges.Provides smooth glossy surfaces free of pinholes and air streaks.Self-lubricating, helps eliminate plate out, improve impact efficiencyIncreases output rates, improves overall efficiency in extruders and calenders
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved