Material Notes:
UNINOX PA-401 is a high molecular weight MMSAN (methyl methacrylate-styrene-acrylonitrile) processing aid. It is a cost effective processing aid for rigid PVC compounds such as calendered sheet, extrusion profile and rigid foam extrusion.Information provided by Pau Tai Industrial Corp.Advantages: Increases melt strength and elasticityImproves thermoforming controlReduces PVC fusion time and gate bilsh in injection moldingImproves rigid PVC foam cell structure
Physical Properties Metric English Comments
Bulk Density 0.220 - 0.420 g/cc
0.00795 - 0.0152 lb/in³
Volatiles <= 1.0 %
<= 1.0 %
Particle Mesh Size 35 Mesh
35 Mesh
2%
Descriptive Properties Value Comments
Appearance White Powder
Dosage, phr 1.0-5.0