Pau Tai Cadmium stearate, Monomer Stabilizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Cadmium stearate, Monomer Stabilizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Transparent heat resistance stabilizer. Excellent effect if used with barium and tin series stabilizer. Excellent lubricant at high temperature operation.Applications: Rigid processing, adhesive plaster, rubber and tube etc..
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Thermal Properties Metric English Comments
Melting Point 103 - 110 °C
217 - 230 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Appearance White micropowder
Metal Content % 17+/- 0.5%