Pasargad Polymer Peyvand Pasalen 3P-H3240B Polypropylene, 40% Mineral Filled Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Pasargad Polymer Peyvand
Trade Name Pasalen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pasargad Polymer Peyvand Pasalen 3P-H3240B Polypropylene, 40% Mineral Filled Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ISO 527-2
Elongation at Break 40 %
40 %
ISO 527-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
Unannealed; ISO 75-2/C
Descriptive Properties Value Comments
Color Black