Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.Parylene is a generic name for poly-para-xylylene polymers used as conformal coatings in protective applications.The coating process exposes objects to the gas-phase monomer at low pressure. Through vacuum deposition, Parylene condenses on the surface in a polycrystalline fashion, providing a coating that is truly conformal and pinhole free.Compared to liquid processes, the effects of gravity and surface tension are negligible -- so there is no bridging, thin-out, pinholes, puddling, run-off or sagging. And, since the process takes place at room temperature, there is no thermal or mechanical stress on the object.Parylene is physically stable and chemically inert within its usable temperature range. Parylene provides excellent protection from moisture, salt spray, corrosive vapors, solvents, airborne contaminants and other hostile environments.Property data obtained following ASTM methods. Information provided by Parylene Coating Services, Inc. (PCS)
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Water Absorption 0.010 %
0.010 %
0.019 inches; 24 hrs.
Moisture Vapor Transmission 0.591 cc-mm/m²-24hr-atm
1.50 cc-mil/100 in²-24hr-atm
37°C; 90% RH
Oxygen Transmission 11.8 cc-mm/m²-24hr-atm
30.0 cc-mil/100 in²-24hr-atm
23°C
Nitrogen Transmission 3.03 cc-mm/m²-24hr-atm
7.70 cc-mil/100 in²-24hr-atm
23°C
Carbon Dioxide Transmission 84.3 cc-mm/m²-24hr-atm
214 cc-mil/100 in²-24hr-atm
23°C
Hydrogen Sulfide Transmission 313 cc-mm/m²-24hr-atm
795 cc-mil/100 in²-24hr-atm
23°C
Sulfur Dioxide Transmission 0.744 cc-mm/m²-24hr-atm
1.89 cc-mil/100 in²-24hr-atm
23°C
Chlorine Transmission 29.1 cc-mm/m²-24hr-atm
74.0 cc-mil/100 in²-24hr-atm
23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
Tensile Strength, Yield 43.4 MPa
6300 psi
Elongation at Break 40 %
40 %
Elongation at Yield 2.5 %
2.5 %
Tensile Modulus 2.40 GPa
348 ksi
Coefficient of Friction, Dynamic 0.25
0.25
Coefficient of Friction, Static 0.25
0.25
Thermal Properties Metric English Comments
CTE, linear 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.120 W/m-K
0.833 BTU-in/hr-ft²-°F
Melting Point 410 °C
770 °F
Optical Properties Metric English Comments
Refractive Index 1.661
1.661
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
50% RH
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
50% RH
Dielectric Constant 2.65

@Frequency 60 Hz
2.65

@Frequency 60 Hz
2.65

@Frequency 1000 Hz
2.65

@Frequency 1000 Hz
2.65

@Frequency 1e+6 Hz
2.65

@Frequency 1e+6 Hz
Dielectric Strength 276 kV/mm
7000 kV/in
Short Time; 1 mil
Dissipation Factor 0.00020

@Frequency 60 Hz
0.00020

@Frequency 60 Hz
0.00020

@Frequency 1000 Hz
0.00020

@Frequency 1000 Hz
0.00060

@Frequency 1e+6 Hz
0.00060

@Frequency 1e+6 Hz
Users viewing this material also viewed the following: