Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material

Category Ceramic , Nitride , Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-THERM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of CHO-THERM® 1646 materials approximates that of thermal grease. One-component CHO-THERM® 1646 pads eliminate the need for grease dispensing equipment or the labor-intensive application process. CHO-THERM® 1646 materials consist of boron nitride-filled silicone coated on one side of .002 in (.05 mm) aluminum foil. Acrylic pressure sensitive adhesive is on the other side of the foil.Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 130 microns
5.12 mil
Mechanical Properties Metric English Comments
Tensile Strength 34.5 MPa
5000 psi
ASTM D412
Tear Strength 30.7 kN/m
175 pli
ASTM D624
Peel Strength 0.180 kN/m
1.03 pli
to Aluminum; ASTM D1876
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
MIL-I-49456a
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Binder Silicone
Carrier Aluminum
Color White/Silver
Filler Boron Nitride
Users viewing this material also viewed the following: