Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Biological, and Chemical requirements. These gaskets are available in continuous extruded profiles for EMI gasketing of large areas.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 2.00 g/cc
>= 2.00 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 87
73 - 87
ASTM D2240
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 12.26 kN/m
69.96 pli
Compression Set 40 %
40 %
70 hrs @ 100°C; D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.050 ohm-cm
0.050 ohm-cm
as supplied (without psa); MIL-G-83528
Shielding Effectiveness >= 90 dB
>= 90 dB
20MHz - 10GHz; MIL-G-83528
Descriptive Properties Value Comments
Binder EPDM
EMP Survivability kA / in, min 0.05
Filler Ag/Ni
Grade Military-Aerospace
Heat Aging ohm-cm max 0.05
Vibration Resistance, After, ohm-cm max 0.05
Vibration Resistance, During, ohm-cm max 0.05