Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-MASK II HT Conductive Foil Tape

Category Polymer , Tape
Manufacturer Parker Chomerics
Trade Name CHO-MASK II
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-MASK II HT Conductive Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MASK II tapes consist of recessed polyester paint masking film covering a layer of either 1 oz. (28.4g) or 2 oz. (56.7g) tinplated copper foil. The back of the foil features a conductive pressure sensitive adhesive (PSA). CHO-MASK II tape is applied to clean metal frame, door and panel surfaces where electrical continuity is required. After painting, the peel-off mask is easily removed, allowing the paint to seal both edges of the foil layer. The foil imparts a clean, electrically conductive path from the panel, through an EMI gasket, to the cabinet frame. It also provides grounding points within the enclosure.Application: Oven bake up to 400°F (204°C) for 1 hour; Suitable for knife edge, radius and flat surface applications; Lengths of
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
1 oz. Tinned Copper Foil
50.8 microns
2.00 mil
Acrylic Adhesive
71.1 microns
2.80 mil
2 oz. Tinned Copper Foil
76.2 microns
3.00 mil
1 oz. Total Thickness; ASTM D1000
122 microns
4.80 mil
2 oz. Total Thickness; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Chomerics
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Chomerics
Electrical Properties Metric English Comments
Surface Resistance <= 0.20 ohm
<= 0.20 ohm
Chomerics TM 71
Processing Properties Metric English Comments
Cure Time <= 60.0 min

@Temperature 204 °C
<= 1.00 hour

@Temperature 399 °F
Paint Cure Cycle
Descriptive Properties Value Comments
Adhesion Mask to Foil 24 oz./inch
ASTM D1000
Adhesion to Aluminum 543 N/m
48 hrs @ 177°C; ASTM D1000
700 N/m
1 hr @ 177°C; ASTM D1000
718 N/m
168 hrs @ 74°C/95% RH; ASTM D1000
893 N/m
1 hr @ 204°C; ASTM D1000
Adhesion to Steel 525 N/m
48 hrs @ 177°C; ASTM D1000
683 N/m
1 hr @ 177°C; ASTM D1000
700 N/m
168 hrs @ 74°C/95% RH; ASTM D1000
875 N/m
1 hr @ 204°C; ASTM D1000
Chemical Resistance Pass
Trichloroethane, ethanol, acids, cleaning solvents, and alkaline solutions; ASTM D896-84
Corrosion Resistance Pass
Salt Fog Chamber at 35°C, 144 hrs; MIL-STD-810
Humidity Exposure Pass
@ 60°C for 96 hours 95% RH; ASTM D1001
Mask Type Polyester