Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease

Category Fluid , Polymer , Adhesive , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-LUBE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHO-LUBE 4220 conductive grease is based on silicone fluid, which is characterized by unusual chemical inertness and outstanding thermal stability. It is a silver-filled lubricant designed for surface-to-surface, particularly metal-to-metal, sliding contact areas requiring continuous electrically conductive paths, such as a switch.It can also be used for grounding of enclosures, equipment or components which require lubrication to overcome friction as well a EMI control. It may be supplied by standard caulking or grease guns.Information provided by Chomerics
Physical Properties Metric English Comments
Density 3.10 g/cc
0.112 lb/in³
Thickness 25.4 microns
1.00 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.519 W/m-K
3.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.10 ohm-cm
0.10 ohm-cm
DC
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Filler Ag
Resin Type Silicone