Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-FORM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material cost versus performance and can provide low cost alternatives for less demanding applications. Chomerics corrosion resistant materials inherently provide protection against galvanic activity. They may eliminate the need for nickel or tin plating and or secondary environmental gaskets. Chomerics general purpose materials exhibit excellent electrical and mechanical properties on metallic and shield plastic housing. Chomerics silver filled materials provide high shielding and conductivity critical for inter-compartmental shields. CHOFORM delivers a greater deflection range, lower deflection forces & improved reliability. Features: Lower deflection forces and a broad deflection range, Corrosion resistant materials can eliminate plating or secondary environmental gasket, Good adhesion to many substrates, Supply chain management providing ongoing logistics, Low cost and rapid prototyping and Corrosion Resistant, Small Bead.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
Deformation 30 %
30 %
49.8 N/cm
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength at Break 2.24 MPa
325 psi
ASTM D412
Elongation at Break 65 %
65 %
ASTM D412
Compression Set 45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 0.050 ohm-cm
0.050 ohm-cm
CHO MAT-1009
Shielding Effectiveness >= 60 dB

@Frequency 200 - 12000 Hz
>= 60 dB

@Frequency 200 - 12000 Hz
Processing Properties Metric English Comments
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH; Tack Free Time
240 min

@Temperature 22.0 °C
4.00 hour

@Temperature 71.6 °F
50% RH; Handling Time
2880 min

@Temperature 22.0 °C
48.0 hour

@Temperature 71.6 °F
50% RH; Full Cure
Shelf Life 5.00 Month

@Temperature 17.0 - 27.0 °C
5.00 Month

@Temperature 62.6 - 80.6 °F
Descriptive Properties Value Comments
Adhesion 9 N/cm
Trivalent Chromate Coating on Aluminum, Chomerics WI 1038
Cure System Moisture
Filler Ni/C
Galvanic Corrosion 10 mg
Resistance Against Aluminum; CHO TM-100
Number of Components 1
Resin System Silicone