Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-FORM 5537 EMI Shielding Material

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-FORM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FORM 5537 EMI Shielding Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-plated graphite particles dispersed in a silicone elastomer.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength at Break >= 1.38 MPa
>= 200 psi
ASTM D412
Compression Set 50 %
50 %
ASTM D395 Method B 22 hrs 85°C
Electrical Properties Metric English Comments
Volume Resistivity 0.020 ohm-cm
0.020 ohm-cm
Initial; Chomerics MAT-1002
0.030 ohm-cm
0.030 ohm-cm
Aged; Chomerics MAT-1002
Processing Properties Metric English Comments
Cure Time 2880 min
48.0 hour
Full Cure
>= 240 min

@Temperature 20.0 °C
>= 4.00 hour

@Temperature 68.0 °F
Minimum Cure time before inspection @ 50% RH
Descriptive Properties Value Comments
Compression/Deflection @ 20%, N/cm 2.1
Compression/Deflection @ 30%, N/cm 4.8
Filler Ni/C
Resin One Part Silicone
Copyright © lookpolymers.com All Rights Reserved