Parker Chomerics CHO-FORM 5519 Conductive Silicone

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-FORM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FORM 5519 Conductive Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Volatiles <= 7.0 %
<= 7.0 %
Component Elements Properties Metric English Comments
Copper, Cu <= 65 %
<= 65 %
Silver, Ag <= 10 %
<= 10 %
Descriptive Properties Value Comments
Color Silver/Gray
Physical Form Silver/gray paste
Silane and Siloxane Compounds wt. % Max 35
Toluene wt. % Max 7