Material Notes:
Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or tinned copper foil backed with Chomerics’ highly conductive pressure-sensitive adhesive.Typical Applications: Provide a low impedance connection between a braided cable shield and the metal connector backshell in molded cables. An effective EMI shielded assembly can be achieved without soldering the tape to the braid or backshell; EMI radiation measurement troubleshooting, using CHO-FOIL tape to shield ventilation slots or seam gaps; Provide electrical continuity in seams of EMI shielded rooms and electronic enclosures; Supply electrical contact to surfaces that can’t be soldered to, such as conductive plastic or aluminum; EMI shield for cables by wrapping the tape around the cable. An overlap is recommended; ESD shielding; Provide corrosion-resistant ground contact points; Fabric tape available where weight and flexibility are important, such as for wrapping cables. Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Foil thickness
76.2 microns
3.00 mil
Adhesive thickness (2-sided)
127 microns
5.00 mil
Total
Mechanical Properties Metric English Comments
Peel Strength 0.771 kN/m
4.40 pli
Initial; ASTM D1000
0.929 kN/m

@Temperature 85.0 °C
5.30 pli

@Temperature 185 °F
95% RH; ASTM D1000
0.841 kN/m

@Temperature 85.0 °C,
Time 605000 sec
4.80 pli

@Temperature 185 °F,
Time 168 hour
ASTM D1000
0.929 kN/m

@Temperature 121 °C,
Time 605000 sec
5.30 pli

@Temperature 250 °F,
Time 168 hour
ASTM D1000
0.877 kN/m

@Time 605000 sec
5.00 pli

@Time 168 hour
Salt fog corrosion; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistance <= 0.10 ohm
<= 0.10 ohm
Initial through resistivity (TR); CHO-TP-57
<= 0.15 ohm

@Temperature 85.0 °C
<= 0.15 ohm

@Temperature 185 °F
95% RH; (TR); CHO-TP-57
<= 0.010 ohm

@Temperature 121 °C,
Time 605000 sec
<= 0.010 ohm

@Temperature 250 °F,
Time 168 hour
(TR); CHO-TP-57
<= 0.060 ohm

@Temperature 85.0 °C,
Time 605000 sec
<= 0.060 ohm

@Temperature 185 °F,
Time 168 hour
(TR); CHO-TP-57
<= 0.60 ohm

@Time 605000 sec
<= 0.60 ohm

@Time 168 hour
Salt fog corrosion; (TR); CHO-TP-57
Surface Resistivity per Square <= 0.010 ohm
<= 0.010 ohm
[ohm/in<sup>2<sup>]; <.0016 ohm/cm<sup>2</sup>; MIL-STD-202C
Descriptive Properties Value Comments
Adhesion to Aluminum >40 oz./inch
ASTM D1000
Adhesive Type Electrically Conductive, Pressure-Sensitive Acrylic
Flame Resistance (UL Subject 510) Meets
Foil/Fabric Type Aluminum