Parker Chomerics CHO-BOND 1073, Part B Conductive Powder

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1073, Part B Conductive Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Carbon Black Loading 100 %
100 %
Descriptive Properties Value Comments
Color Black
Physical Form Black odorless powder.