Parker Chomerics CHO-BOND 1055, Part A Silicone Resin Mixture

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1055, Part A Silicone Resin Mixture.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Carbon Black Loading <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Silver Coated Copper wt. % Max 100