Parker Chomerics CHO-BOND 1011, Part A

Category Polymer , Adhesive , Thermoset
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1011, Part A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Component Elements Properties Metric English Comments
Copper, Cu >= 80 %
>= 80 %
Silver, Ag <= 5.0 %
<= 5.0 %
Descriptive Properties Value Comments
Diatomaceous Earth wt. % Max 5
Physical Form Silver Paste
Silicone Resin % <10