Material Notes:
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized for use with woven aramid reinforcementsMeets requirements of MIL-R-9300B, Type 1Long out-time for easy processingApplications/Qualifications:Military HelicoptersEngine NacellesWork PlatformsDoorsAir FramesInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 3.0 %

@Temperature 135 °C
<= 3.0 %

@Temperature 275 °F
8 min
Mechanical Properties Metric English Comments
Flexural Strength 359 MPa

@Temperature 23.9 °C
52000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 33.1 GPa

@Temperature 23.9 °C
4800 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Shear Strength 32.4 MPa

@Temperature 23.9 °C
4700 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Processing Properties Metric English Comments
Gel Time 1.00 - 6.00 min
1.00 - 6.00 min
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Resin Flow (%) 28-45
325°F, 15psi