Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pacific Sintered Materials FN-252-S Iron Nickel Soft Magnetic Powdered Metal

Category Metal , Ferrous Metal
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials FN-252-S Iron Nickel Soft Magnetic Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Very low coercive force and high permeability. Excellent for shielding and switching applications.All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.00 - 7.20 g/cc
0.253 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 300 MPa
43500 psi
Elongation at Break 10 %
10 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 13.3
<= 13.3
K-Gauss/Oe
Magnetic Coercive Force, Hc 0.40 Oe
0.40 Oe
Magnetic Saturation Flux Density, Bmax 10000 Gauss
10000 Gauss
Magnetic Induction
Magnetic Remanence, Br 7000 Gauss
7000 Gauss
Users viewing this material also viewed the following: