Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pacific Sintered Materials BZ-111-U Yellow Brass Powdered Metal

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials BZ-111-U Yellow Brass Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: 80-20 leaded brass for structural and hardware components.Equivalent MPIF Specification: CZP-2000-11All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.60 - 7.80 g/cc
0.275 - 0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell H 70
70
Tensile Strength, Ultimate 159 MPa
23000 psi
Tensile Strength, Yield 93.1 MPa
13500 psi
Elongation at Break 12 %
12 %
Flexural Strength 345 MPa
50000 psi
Transverse Rupture
Charpy Impact, Unnotched 38.0 J
28.0 ft-lb
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000069 ohm-cm
0.0000069 ohm-cm
Descriptive Properties Value Comments
Electrical Conductivity (% IACS) 25
Users viewing this material also viewed the following: