Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
ASTM D2240
Tensile Strength, Ultimate 14.8 MPa
2150 psi
ASTM D412
Tensile Strength, Yield 0.931 MPa
135 psi
at 100%; ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 24.5 kN/m
140 pli
die C; ASTM D624
Compression Set 55 - 66 %
55 - 66 %
ASTM D395
Users viewing this material also viewed the following: