P & P Technology EPDM Closed Cell Sponge

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer P & P Technology
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology EPDM Closed Cell Sponge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Metweave is a lamination of PPT conductive fabric and closed cell EPDM.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 0.110 - 0.150 g/cc
0.110 - 0.150 g/cc
Water Absorption <= 0.80 %
<= 0.80 %
Vacuum
Deformation 25 %

@Pressure 0.0200 - 0.0400 MPa
25 %

@Pressure 2.90 - 5.80 psi
Compression
50 %

@Pressure 0.0700 - 0.100 MPa
50 %

@Pressure 10.2 - 14.5 psi
Compression
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 55
35 - 55
Tensile Strength 0.220 MPa
31.9 psi
Elongation at Break >= 180 %
>= 180 %
Tear Strength >= 1.00 kN/m
>= 5.71 pli
Compression Set <= 30 %

@Temperature 23.0 °C,
Time 79200 sec
<= 30 %

@Temperature 73.4 °F,
Time 22.0 hour
0.5
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0