Material Notes:
Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core, electronic keyboard contacts, etc.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
DIN 53479-A
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
DIN 53505-A
Tensile Strength 5.70 MPa
827 psi
DIN 53504-S1
Elongation at Break 339 %
339 %
DIN 53504-S1
Tear Strength 10.5 kN/m
59.9 pli
ASTM D624B
Compression Set 32 %
32 %
DIN ISO815-B
Electrical Properties Metric English Comments
Volume Resistivity 6.4 ohm-cm
6.4 ohm-cm
DIN IEC93