Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers Oxnilon 66-43GF 43% Glass Fiber Filled Nylon 66 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 66-43GF 43% Glass Fiber Filled Nylon 66 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
43% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Filler Content 43 %
43 %
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 193 MPa
28000 psi
ASTM D638
Tensile Strength, Yield 190 MPa
27500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
485 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 288 - 304 °C
550 - 580 °F