Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers 30GF 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), 30% Glass Fiber
Manufacturer Oxford Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 30GF 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.16 %
0.16 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 155 MPa
22500 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Temperature 23.0 °C
1.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
414 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 382 °C
720 °F