Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Owens Corning Glass Fiber Reinforced Polyurethane, Flaked Glass (RRIM), 23 wt.% glass

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyurethane, TS
Manufacturer Owens Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polyurethane, Flaked Glass (RRIM), 23 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, and ketones. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.4 MPa
4410 psi
ASTM D638
Elongation at Break 38.9 %
38.9 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 95.6 µm/m-°C

@Temperature 20.0 °C
53.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Flammability, UL94 V-0
V-0
Users viewing this material also viewed the following: