Owens Corning Glass Fiber Reinforced Polystyrene Acrylonitrile (SAN), 20 wt.% glass

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer Owens Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polystyrene Acrylonitrile (SAN), 20 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene provides good resistance to alkalis, most organic solvents, weak acids, and household chemicals. It is not recommended for use with strong acids, ketones, esters, and some chlorinated hydrocarbons (test before use). Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Ultimate 100 MPa
14500 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Modulus of Elasticity 8.62 GPa
1250 ksi
ASTM D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Compressive Strength 121 MPa
17500 psi
ASTM D695
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 60 Hz
3.5

@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.3 kV/mm
490 kV/in
ASTM D149
Arc Resistance 70 sec
70 sec
ASTM D495