Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Owens Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for use with strong alkalis. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ASTM D792
Water Absorption 0.75 %
0.75 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 50
50
Tensile Strength, Ultimate 200 MPa
29000 psi
ASTM D638
Modulus of Elasticity 17.0 GPa
2470 ksi
ASTM D638
Flexural Strength 210 MPa
30500 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 200 MPa
29000 psi
ASTM D695
Izod Impact, Notched 13.0 J/cm
24.4 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 20.0 °C
5.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Thermal Conductivity 0.576 W/m-K
4.00 BTU-in/hr-ft²-°F
ASTM C177
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.4

@Frequency 60 Hz
4.4

@Frequency 60 Hz
ASTM D150
Dielectric Strength 7.87 kV/mm
200 kV/in
ASTM D149
Arc Resistance 80 sec
80 sec
ASTM D495