Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Owens Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene dichloride. Acetal is highly resistant to strong alkalis. Most organic solvents do not seriously alter its properties (test before use). It is not recommended for use in strong acids. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Modulus of Elasticity 6.00 GPa
870 ksi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Compressive Strength 97.0 MPa
14100 psi
ASTM D695
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 60 Hz
3.2

@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.3 kV/mm
465 kV/in
ASTM D149
Arc Resistance 80 sec
80 sec
ASTM D495