Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid, Quartz Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.69 - 1.80 g/cc
0.0611 - 0.0650 lb/in³
Average value: 1.75 g/cc Grade Count:3
Water Absorption 0.0500 - 0.0900 %
0.0500 - 0.0900 %
Average value: 0.0667 % Grade Count:3
Water Absorption at Saturation 0.0500 - 0.0900 %
0.0500 - 0.0900 %
Average value: 0.0667 % Grade Count:3
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.0 - 88.0 MPa
10900 - 12800 psi
Average value: 82.3 MPa Grade Count:3
Elongation at Break 1.10 - 1.40 %
1.10 - 1.40 %
Average value: 1.27 % Grade Count:3
Modulus of Elasticity 8.00 - 9.10 GPa
1160 - 1320 ksi
Average value: 8.70 GPa Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 34.0 - 42.0 µm/m-°C
18.9 - 23.3 µin/in-°F
Average value: 38.7 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 34.0 - 42.0 µm/m-°C
18.9 - 23.3 µin/in-°F
Average value: 38.7 µm/m-°C Grade Count:3
Glass Transition Temp, Tg 90.0 - 140 °C
194 - 284 °F
Average value: 123 °C Grade Count:3
Oxygen Index 29.0 - 51.0 %
29.0 - 51.0 %
Average value: 38.3 % Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 8.00e+14 - 1.00e+15 ohm-cm
8.00e+14 - 1.00e+15 ohm-cm
Average value: 9.33e+14 ohm-cm Grade Count:3
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Average value: 1.00e+15 ohm Grade Count:3
Dielectric Constant 4.00 - 4.70
4.00 - 4.70
Average value: 4.38 Grade Count:3
Dielectric Strength 29.0 - 34.0 kV/mm
737 - 864 kV/in
Average value: 31.7 kV/mm Grade Count:3
Dissipation Factor 0.0100 - 0.0250
0.0100 - 0.0250
Average value: 0.0145 Grade Count:3
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:3