Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon + Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.30 - 1.38 g/cc
0.0470 - 0.0499 lb/in³
Average value: 1.34 g/cc Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00150 cm/cm Grade Count:3
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 - 143 MPa
18200 - 20700 psi
Average value: 133 MPa Grade Count:3
Elongation at Break 2.00 - 4.00 %
2.00 - 4.00 %
Average value: 3.17 % Grade Count:3
Modulus of Elasticity 8.69 - 13.0 GPa
1260 - 1890 ksi
Average value: 10.5 GPa Grade Count:3
Flexural Yield Strength 192 - 199 MPa
27900 - 28800 psi
Average value: 195 MPa Grade Count:3
Flexural Modulus 8.62 - 11.9 GPa
1250 - 1730 ksi
Average value: 9.85 GPa Grade Count:3
Izod Impact, Notched 1.20 - 1.31 J/cm
2.25 - 2.45 ft-lb/in
Average value: 1.25 J/cm Grade Count:3
Processing Properties Metric English Comments
Melt Temperature 288 - 316 °C
550 - 601 °F
Average value: 303 °C Grade Count:3
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Average value: 103 °C Grade Count:3
Drying Temperature 121 - 121 °C
250 - 250 °F
Average value: 121 °C Grade Count:3