Ovation Polymers SOFTAPLAS™ R 60300 GF Nat Thermoplastic Polyurethane, 30% Glass Fiber

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer Ovation Polymers
Trade Name SOFTAPLAS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers SOFTAPLAS™ R 60300 GF Nat Thermoplastic Polyurethane, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% short glass fiber reinforced for excellent strength and processabilityAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
50 mm/min; ASTM D638
Elongation at Break 13 %
13 %
50 mm/min; ASTM D638
Tensile Modulus 2.45 GPa
355 ksi
50 mm/min; ASTM D638
Flexural Strength 90.0 MPa
13100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.75 GPa
399 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.94 J/cm

@Temperature 23.0 °C
5.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C

@Thickness 3.20 mm
172 °F

@Thickness 0.126 in
Unannealed; ASTM D648