Material Notes:
PET – 25% Short Glass Fiber Reinforced with Flame retardant. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 98.0 MPa
14200 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Tensile Modulus 5.50 GPa
798 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 150 MPa
21800 psi
1.3 mm/min; ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 170 °C

@Thickness 3.20 mm
338 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0