Material Notes:
PBT - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Linear Mold Shrinkage 0.0035 - 0.0045 cm/cm
0.0035 - 0.0045 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
50 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
50 mm/min; ASTM D638
Tensile Modulus 4.60 GPa
667 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 125 MPa
18100 psi
1.3 mm/min; ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C

@Thickness 3.20 mm
360 °F

@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 °C

@Thickness 3.20 mm
338 °F

@Thickness 0.126 in
ASTM D648