Material Notes:
PC - Glass reinforced (20 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Melt Index of Compound 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 92.9 MPa
13500 psi
50 mm/min; ASTM D638
Elongation at Break 3.5 %
3.5 %
50 mm/min; ASTM D638
Tensile Modulus 3.60 GPa
522 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 132 MPa
19100 psi
1.3 mm/min; ASTM D790
Flexural Modulus 5.40 GPa
783 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 3.20 mm
273 °F

@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 3.20 mm
264 °F

@Thickness 0.126 in
ASTM D648