Ovation Polymers RIGITRON 10001 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers RIGITRON 10001 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC – Impact Modified, high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0040 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0010 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0010 - 0.0040 in/in

@Thickness 0.125 in
Melt Index of Compound 15 - 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
15 - 18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
50 mm/min; ASTM D638
Elongation at Break 20 %
20 %
50 mm/min; ASTM D638
Tensile Modulus 1.85 GPa
268 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
1.3 mm/min; ASTM D790
Flexural Modulus 2.25 GPa
326 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 6.941 J/cm
13.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
ASTM D648