Ovation Polymers OpteSTAT™ NC PES 6010 Polyether Sulfone based Carbon Nanotube Compound

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone, Carbon Fiber Reinforced
Manufacturer Ovation Polymers
Trade Name OpteSTAT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers OpteSTAT™ NC PES 6010 Polyether Sulfone based Carbon Nanotube Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or other electronic assemblies where ESD control is required while retaining exceptional cleanliness, dimensional control and physical propertiesAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
50 mm/min; ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
50 mm/min; ASTM D638
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C

@Thickness 3.20 mm
295 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257