Ovation Polymers Nemcon™ E ABS 20CF

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E ABS 20CF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E ABS 20CF is a high modulus carbon fiber-reinforced ABS with excellent conductivity. It is suitable for a wide variety of injection molding applications, including electronic components, shipping trays, storage racks, electronic housings and work surfaces. Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.129 g/cc
1.129 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
50 mm/min; ASTM D638
Elongation at Break 1.9 %
1.9 %
50 mm/min; ASTM D638
Tensile Modulus 10.5 GPa
1520 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 128 MPa
18600 psi
1.3 mm/min; ASTM D790
Flexural Modulus 9.535 GPa
1383 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.459 J/cm

@Temperature 23.0 °C
0.860 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 2750 ohm
2750 ohm
ASTM D257