Material Notes:
A dry ground, high whiteness calcium carbonate with tightly controlled top size.Applications: Aggregate for stucco and swimming pool plaster.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.71 g/cc
2.71 g/cc
Brightness 90 %
90 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.030 %
0.030 %
Moisture Loss at 110°C % (dry)
Particle Size 350 µm
350 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 95
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 1.5
Retained in 200 mesh, (dry) % 90
Retained in 40 mesh % 30