Material Notes:
A dry ground calcium carbonate with an intermediate particle distribution, unique size, color, and purity.Applications: Ideal for cementitious grouts, plasters, and automotive underspray applications.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.71 g/cc
2.71 g/cc
Brightness 94 %
94 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.030 %
0.030 %
Moisture Loss at 110°C % (dry)
Particle Size 16 µm
16 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 93
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 3
Retained in 325 mesh (dry) ppm 15