Omya SNOWHITE® 12-40 - PT Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name SNOWHITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya SNOWHITE® 12-40 - PT Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A bright white, dry screen-separated grade.Applications: Concrete matrix and mortar sand; ASTM golf bunker sand.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.71 g/cc
2.71 g/cc
Brightness 84 %
84 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.050 %
0.050 %
Moisture Loss at 110°C % (dry)
Descriptive Properties Value Comments
Calcium Carbonate % 94
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 2
Retained in 40 mesh % 80
Retained in 50 mesh, ppm % 83