Omya OMYACARB® 5 - FL Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYACARB®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYACARB® 5 - FL Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A beneficiated calcium carbonate with an intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated polyester compounds (SMC, BMC, TMC). Also used in paint applications.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
dry
Brightness 95 %
95 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.040 %
0.040 %
Moisture Loss at 110°C % (dry)
Particle Size 6.0 µm
6.0 µm
Median Diameter
Specific Surface Area 2.1 m²/g
2.1 m²/g
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
dry
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 5
Magnesium Carbonate % 1
Pounds Pigment/Solid Gallon (dry) 22.6
Retained in 325 mesh (dry) ppm 140