Omya HYDROCARB® 60 Calcium Carbonate

Category Ceramic
Manufacturer Omya North America
Trade Name HYDROCARB®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya HYDROCARB® 60 Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A fine ground calcium carbonate for paper and board coating.Information supplied by Omya North America.
Physical Properties Metric English Comments
Solids Content 73.5 %
73.5 %
Slurry Solids
Brightness 97 %
97 %
T534 om-76 Brightness (Diffuse Reflectance)
Loss On Ignition 0.000 %

@Temperature 400 °C
0.000 %

@Temperature 752 °F
42.6 %

@Temperature 900 °C
42.6 %

@Temperature 1650 °F
Particle Size 1.4 µm
1.4 µm
Median Diameter
Specific Surface Area 7.0 m²/g
7.0 m²/g
Brookfield Viscosity 200 cP

@Temperature 25.0 °C
200 cP

@Temperature 77.0 °F
No. 3 Spindle, 100 rpm
Optical Properties Metric English Comments
Reflection Coefficient, Visible (0-1) 0.97
0.97
T534 om-76 Brightness (Diffuse Reflectance)
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 176.170, 176.180
Magnesium Carbonate % 1