Omnia Plastica Noryl® PPO m Polyphenylenoxide

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded , Polystyrene (PS)
Manufacturer Omnia Plastica s.p.a.
Trade Name Noryl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omnia Plastica Noryl® PPO m Polyphenylenoxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl is a resin based on polyphenylene oxide, modified with styrene. Its main field of application is the electrical one.Features:Good electrical properties, even at high frequency Dimensional stability, low moisture absorption Excellent stability Gamma ray resistance Colour greyWeak Point:It has poor mechanical featuresApplication:Electrical: Used particularly for its electrical properties. Suitable for high frequency insulators and components in the electronic industry. Mechanical: It has poor mechanical properties. Good gamma ray resistance. Food contact: It is not used in contact with food. Chemical: The resistance is poor and it is not used for chemical applications.Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.10 %
0.10 %
50% relative humidity
Water Absorption at Saturation 0.30 %
0.30 %
23°C
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
dry sample; ISO2039.2
Ball Indentation Hardness 100 MPa
14500 psi
ISO2039.1 DIN.53456
Tensile Strength at Break 45.0 MPa
6530 psi
ISO.527 DIN.53455
Elongation at Break 60 %
60 %
ISO.527 DIN.53455
Tensile Modulus 2.30 GPa
334 ksi
ISO.527 DIN.53455
Compressive Strength 16.0 MPa
2320 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB
NB
7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.50
0.50
on dry ground steel; load =0.05MPa; speed =0.6 m/s
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
33.3 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
DIN.52612
Maximum Service Temperature, Air 90.0 °C
194 °F
Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C.
105 °C
221 °F
short period, no load
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO.75 DIN.53461
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
impact conditions and heavy loads not considered
Flammability, UL94 HB
HB
Oxygen Index 26 %
26 %
ISO.4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ISO.93 DIN.53482
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 22.0 kV/mm
559 kV/in
ISO.243 DIN.53481
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
ISO.250 DIN.53483
Descriptive Properties Value Comments
Form Amorphous
Copyright © lookpolymers.com All Rights Reserved