Omni Plastics OmniTuff™ HPP CCF20 Homopolymer Polypropylene Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Omni Plastics
Trade Name OmniTuff™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTuff™ HPP CCF20 Homopolymer Polypropylene Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256