Material Notes:
No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high percentage of frit which has soluble alkali. No. Glaze provides viscosity control range and excellent rheology for all glaze application methods and especially bell or cone applications processes.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Particle Size 0.37 µm
0.37 µm
Median particle diameter
0.50 µm
0.50 µm
52% of particles less than
1.0 µm
1.0 µm
63% of particles less than
<= 5.0 µm
<= 5.0 µm
87% of particles less than
pH 5.9
5.9
Soluble Sulfates 160 ppm
160 ppm
Specific Surface Area 18 m²/g
18 m²/g
Thermal Properties Metric English Comments
CTE, linear 5.90 µm/m-°C

@Temperature 50.0 - 500 °C
3.28 µin/in-°F

@Temperature 122 - 932 °F
Pre-fired 1200°C
Shrinkage 5.8 %
5.8 %
Linear Drying Shrinkage
Component Elements Properties Metric English Comments
Al2O3 29.37 %
29.37 %
CaO 0.10 %
0.10 %
Carbon, C 0.080 %
0.080 %
Fe2O3 0.87 %
0.87 %
K2O 0.28 %
0.28 %
Kaolinite 70.8 %
70.8 %
Loss on Ignition(%) 9.91 %
9.91 %
MgO 0.28 %
0.28 %
Na2O 0.10 %
0.10 %
Quartz 22.4 %
22.4 %
SiO2 56.32 %
56.32 %
Sulfur, S 0.000073 %
0.000073 %
TiO2 2.44 %
2.44 %
Descriptive Properties Value Comments
CEC/MBI (meg/100 ml) 7.1
Crude Color White
Dry Sieve Residue (%) 0.4
Dry Sieve Residue, +80 mesh
Feldspar (%) 4.8
Misc. Trace Minerals (%) 2.3
Nature of Residue High Purity Quartz
Water of Plasticity (%) 31
Wet Sieve Residue (%) 0.34
Wet Sieve Residue, +325 mesh
0.39
Wet Sieve Residue, +200 mesh
Users viewing this material also viewed the following: